WO2025114949 - POLYETHYLENE ROTOMOLDING COMPOSITION HAVING IMPROVED ADHESION PROPERTIES TO POLYURETHANE

National phase entry is expected:
Publication Number WO/2025/114949
Publication Date 05.06.2025
International Application No. PCT/IB2024/062007
International Filing Date 28.11.2024
Title **
[English] POLYETHYLENE ROTOMOLDING COMPOSITION HAVING IMPROVED ADHESION PROPERTIES TO POLYURETHANE
[French] COMPOSITION DE ROTOMOULAGE DE POLYÉTHYLÈNE DOTÉE DE PROPRIÉTÉS D'ADHÉRENCE AU POLYURÉTHANE AMÉLIORÉES
Applicants **
NOVA CHEMICALS (INTERNATIONAL) S.A.
Inventors
WASYLENKO, Derek
D'AGOSTINO, Carmine
Priority Data
63/605,253   01.12.2023   US
Application details
Total Number of Claims/PCT *
Number of Independent Claims *
Number of Priorities *
Number of Multi-Dependent Claims *
Number of Drawings *
Pages for Publication *
Number of Pages with Drawings *
Pages of Specification *
*
Number of Office Actions *
*
International Searching Authority
*
Recordal of a Change of the Applicant's Name/Address
*
Type of Assignment
*
Applicant's Legal Status
*
*
*
*
*
*
Entry into National Phase under
*
Patent Delivery
*
Translation

* The data is based on automatic recognition. Please verify and amend if necessary.

** IP-Coster compiles data from publicly available sources. If this data includes your personal information, you can contact us to request its removal.

Quotation for National Phase entry

Country StagesTotal
China Filing, Examination, Granting2498
EPO Filing, Examination, Granting15465
Japan Filing, Examination, Granting2584
South Korea Filing, Examination, Granting2951
USA Filing, Examination, Granting7740
MasterCard Visa
Total: 31,238

The term for entry into the National Phase has expired. This quotation is for informational purposes only

Contact Us
Abstract[English] A rotomolding composition and a method of rotational molding are disclosed. The rotomolding composition can include (a) 85 wt. % to 99 wt. %, based on the total weight of the rotomolding composition, of a first particulate polyethylene composition having an average particle size of 300 microns to 1500 microns; and (b) 1 wt. % to 15 wt. %, based on the total weight of the rotomolding composition, of a second particulate polyethylene composition that includes 500 ppm to 5000 ppm, based on the total weigh of the second particulate polyethylene composition, of a transition metal stearate, and at least 100 parts per million (ppm), based on the total weight of the second particulate polyethylene composition, of an antioxidant, where the second particulate polyethylene composition has an average particle size of 300 microns to 1500 microns.[French] Une composition de rotomoulage et un procédé de moulage rotatif sont divulgués. La composition de rotomoulage peut comprendre (a) 85 % en poids à 99 % en poids, sur la base du poids total de la composition de rotomoulage, d'une première composition de polyéthylène particulaire présentant une taille moyenne de particule de 300 microns à 1 500 microns ; et (b) 1 % en poids à 15 % en poids, sur la base du poids total de la composition de rotomoulage, d'une seconde composition de polyéthylène particulaire qui comprend 500 ppm à 5 000 ppm, sur la base du poids total de la seconde composition de polyéthylène particulaire, d'un stéarate de métal de transition, et au moins 100 parties par million (ppm), sur la base du poids total de la seconde composition de polyéthylène particulaire, d'un antioxydant, la seconde composition de polyéthylène particulaire présentant une taille moyenne de particule de 300 microns à 1 500 microns.