WO2024189533 - MAKING CATALYSTS FOR OXIDATIVE DEHYDROGENATION

National phase entry:
Publication Number WO/2024/189533
Publication Date 19.09.2024
International Application No. PCT/IB2024/052374
International Filing Date 12.03.2024
Title **
[English] MAKING CATALYSTS FOR OXIDATIVE DEHYDROGENATION
[French] FABRICATION DE CATALYSEURS DESTINÉS À LA DÉSHYDROGÉNATION OXYDATIVE
Applicants **
NOVA CHEMICALS (INTERNATIONAL) S.A. Avenue de la Gare 14 1700 Fribourg, CH
Inventors
TAYLOR, Jared c/o NOVA Chemicals Centre for Applied Research 2928 - 16th Street NE Calgary, Alberta T2E 7K7, CA
Priority Data
63/489,897   13.03.2023   US
Application details
Total Number of Claims/PCT *
Number of Independent Claims *
Number of Priorities *
Number of Multi-Dependent Claims *
Number of Drawings *
Pages for Publication *
Number of Pages with Drawings *
Pages of Specification *
*
*
International Searching Authority
*
Applicant's Legal Status
*
*
*
*
*
Entry into National Phase under
*
Translation

Recalculate

* The data is based on automatic recognition. Please verify and amend if necessary.

** IP-Coster compiles data from publicly available sources. If this data includes your personal information, you can contact us to request its removal.

Quotation for National Phase entry

Country StagesTotal
China Filing1503
EPO Filing, Examination8832
Japan Filing531
South Korea Filing575
USA Filing, Examination4035
MasterCard Visa

Total: 15476

The term for entry into the National Phase has expired. This quotation is for informational purposes only

Abstract[English] Methods for preparing a catalyst are provided. An exemplary method includes forming a slurry including metal oxides, a reducing agent, and water; and heating the slurry to form the catalyst. The metal oxides include an oxide of molybdenum; an oxide of vanadium; an oxide of tellurium or an oxide of antimony, or both; and an oxide of tantalum 5 or an oxide of niobium, or both. A ratio of the water in the slurry to amount of catalyst formed is between 0.1 mL water per gram of catalyst and 10 mL water per gram of catalyst.[French] L'invention concerne des procédés de préparation d'un catalyseur. Un procédé donné à titre d'exemple comprend la formation d'une suspension comprenant des oxydes métalliques, un agent réducteur et de l'eau ; et le chauffage de la suspension pour former le catalyseur. Les oxydes métalliques comprennent un oxyde de molybdène ; un oxyde de vanadium ; un oxyde de tellure ou un oxyde d'antimoine, ou les deux ; et un oxyde de tantale ou un oxyde de niobium, ou les deux. Un rapport de l'eau dans la suspension à la quantité de catalyseur formée est compris entre 0,1 mL d'eau par gramme de catalyseur et 10 mL d'eau par gramme de catalyseur.