WO2026132963 - NEAR SOLIDUS FORMING PROCESS TO COMPACT SWARF OR POWDER TO PRODUCE METALLIC COMPONENTS

National phase entry is expected:
Publication Number WO/2026/132963
Publication Date 25.06.2026
International Application No. PCT/IB2025/062313
International Filing Date 02.12.2025
Title **
[English] NEAR SOLIDUS FORMING PROCESS TO COMPACT SWARF OR POWDER TO PRODUCE METALLIC COMPONENTS
[French] PROCÉDÉ DE FORMATION PROCHE DE SOLIDUS DE COPEAUX COMPACTS OU DE POUDRE POUR PRODUIRE DES COMPOSANTS MÉTALLIQUES
Applicants **
NEAR SOLIDUS FORMING TECHNOLOGIES S.L.
Inventors
PLATA, Gorka
SLATER, Carl
LOZARES, Jokin
Priority Data
63/734,248   16.12.2024   US
Application details
Total Number of Claims/PCT *
Number of Independent Claims *
Number of Priorities *
Number of Multi-Dependent Claims *
Number of Drawings *
Pages for Publication *
Number of Pages with Drawings *
Pages of Specification *
*
Number of Office Actions *
*
International Searching Authority
*
Recordal of a Change of the Applicant's Name/Address
*
Type of Assignment
*
Applicant's Legal Status
*
*
*
*
*
*
Entry into National Phase under
*
Patent Delivery
*
译文

* The data is based on automatic recognition. Please verify and amend if necessary.

** IP-Coster compiles data from publicly available sources. If this data includes your personal information, you can contact us to request its removal.

Quotation for National Phase entry

Country StagesTotal
China Filing, Examination, Granting2200
EPO Filing, Examination, Granting11166
Japan Filing, Examination, Granting2339
South Korea Filing, Examination, Granting2442
USA Filing, Examination, Granting4940
MasterCard Visa
Total: 23,087
Contact Us
Abstract[English] A method for hot-shaping metal swarf or powder, the method comprises heating the metal swarf or powder to an intermediate temperature between the metal swarf or powder material hot forging temperature and above the beginning of the melting of said metal swarf or powder material or above the solidus temperature of said metal swarf or powder material, performing forging of said metal swarf or powder and cooling the resulting forged metal part, wherein the forging is performed at temperatures between 150 - 100 ºC below the solidus temperature, Ts, of the metal swarf or powder material and a 20% of liquid fraction of the metal swarf or powder material and wherein the forging is performed in a closed die tooling.[French] L'invention concerne un procédé de formage à chaud de copeaux ou de poudre de métal, le procédé comprenant le chauffage du copeau ou de la poudre de métal jusqu'à une température intermédiaire entre la température de forgeage à chaud du matériau en copeaux ou en poudre de métal et au-dessus du début de la fusion dudit matériau en copeaux ou en poudre de métal ou au-dessus de la température de solidus dudit matériau en copeaux ou en poudre de métal, la réalisation d'un forgeage dudit copeau ou poudre de métal et le refroidissement de la pièce métallique forgée ainsi obtenue, le forgeage étant effectué à des températures comprises entre 150 et 100 °C au-dessous de la température de solidus, Ts, du matériau en copeaux ou en poudre de métal et un 20 % de fraction liquide du du matériau en copeaux ou en poudre de métal et le forgeage étant effectué dans un outillage à matrice fermée.