WO2025257743 - ELECTRICALLY CONDUCTIVE POLYETHYLENE COMPOUNDS HAVING IMPROVED PROPERTIES

National phase entry is expected:
Publication Number WO/2025/257743
Publication Date 18.12.2025
International Application No. PCT/IB2025/055947
International Filing Date 10.06.2025
Title **
[English] ELECTRICALLY CONDUCTIVE POLYETHYLENE COMPOUNDS HAVING IMPROVED PROPERTIES
[French] COMPOSÉS DE POLYÉTHYLÈNE ÉLECTRIQUEMENT CONDUCTEURS AYANT DES PROPRIÉTÉS AMÉLIORÉES
Applicants **
SHPP GLOBAL TECHNOLOGIES B.V.
Inventors
SILVI, Norberto
Priority Data
24181325.2   11.06.2024   EP
Application details
Total Number of Claims/PCT *
Number of Independent Claims *
Number of Priorities *
Number of Multi-Dependent Claims *
Number of Drawings *
Pages for Publication *
Number of Pages with Drawings *
Pages of Specification *
*
Number of Office Actions *
*
International Searching Authority
*
Recordal of a Change of the Applicant's Name/Address
*
Type of Assignment
*
Applicant's Legal Status
*
*
*
*
*
*
Entry into National Phase under
*
Patent Delivery
*
译文

* The data is based on automatic recognition. Please verify and amend if necessary.

** IP-Coster compiles data from publicly available sources. If this data includes your personal information, you can contact us to request its removal.

Quotation for National Phase entry

Country StagesTotal
China Filing, Examination, Granting2034
EPO Filing, Examination, Granting8203
Japan Filing, Examination, Granting2122
South Korea Filing, Examination, Granting2008
USA Filing, Examination, Granting4740
MasterCard Visa
Total: 19,107
Contact Us
Abstract[English] /g) as determined in accordance with ASTM D3037, an oil absorption number (OAN) of at most 300 ml/ 100g as determined in accordance with ASTM D2414, and an iodine absorption of at most 600 mg/g as determined in accordance with ASTM D1510. The composition has a volume electrical resistivity of at most 1.65 ohm. centimeter (ohm.cm), and a capillary melt viscosity of at most 3300 Pascal-seconds (Pa s) at a temperature of 280 °C and a shear rate of 100 reciprocal seconds (1/s).[French] /g) telle que déterminée conformément à la norme ASTM D3037, un indice d'absorption d'huile (OAN) d'au plus 300 ml/100 g tel que déterminé conformément à la norme ASTM D2414, et une absorption d'iode d'au plus 600 mg/g telle que déterminée conformément à la norme ASTM D1510. La composition présente une résistivité électrique volumique d'au plus 1,65 ohm-centimètre (ohm-cm), et une viscosité à l'état fondu capillaire d'au plus 3300 Pascal secondes (Pa s) à une température de 280 °C et un taux de cisaillement de 100 secondes réciproques (1/s).