WO2023139512 - METHOD OF ADJUSTING ELECTRICAL PROPERTIES BY SILICA IN THERMOPLASTIC COMPOSITIONS AND USES THEREOF

National phase entry:
Publication Number WO/2023/139512
Publication Date 27.07.2023
International Application No. PCT/IB2023/050459
International Filing Date 19.01.2023
Title **
[English] METHOD OF ADJUSTING ELECTRICAL PROPERTIES BY SILICA IN THERMOPLASTIC COMPOSITIONS AND USES THEREOF
[French] PROCÉDÉ DE RÉGLAGE DE PROPRIÉTÉS ÉLECTRIQUES PAR DE LA SILICE DANS DES COMPOSITIONS THERMOPLASTIQUES ET LEURS UTILISATIONS
Applicants **
SHPP GLOBAL TECHNOLOGIES B.V.
Inventors
GUO, Mingcheng
ZHANG, Shen
Priority Data
22152418.4   20.01.2022   EP
Application details
Total Number of Claims/PCT *
Number of Independent Claims *
Number of Priorities *
Number of Multi-Dependent Claims *
Number of Drawings *
Pages for Publication *
Number of Pages with Drawings *
Pages of Specification *
*
Number of Office Actions *
*
International Searching Authority
*
Recordal of a Change of the Applicant's Name/Address
*
Type of Assignment
*
Applicant's Legal Status
*
*
*
*
*
*
Entry into National Phase under
*
Patent Delivery
*
译文

* The data is based on automatic recognition. Please verify and amend if necessary.

** IP-Coster compiles data from publicly available sources. If this data includes your personal information, you can contact us to request its removal.

Quotation for National Phase entry

Country StagesTotal
China Filing, Examination, Granting2093
EPO Filing, Examination, Granting8366
Japan Filing, Examination, Granting2155
South Korea Filing, Examination, Granting2071
USA Filing, Examination, Granting4740
MasterCard Visa
Total: 19,425

The term for entry into the National Phase has expired. This quotation is for informational purposes only

Contact Us
Abstract[English] Ohm/square when tested in accordance with ASTM D257, wherein the combined weight percent value of all components does not exceed 100 wt. %, and all weight percent values are based on the total weight of the composition.[French] Ohm/carré lorsqu'elle est testée conformément à la norme ASTM D257, la valeur de pourcentage en poids combinée de tous les composants ne dépassant pas 100 % en poids, et toutes les valeurs de pourcentage en poids étant basées sur le poids total de la composition.