WO2025241464 - PREPARATION METHOD FOR BIO-BASED POLYURETHANE ELASTIC FIBER
National phase entry is expected:
Publication Number
WO/2025/241464
Publication Date
27.11.2025
International Application No.
PCT/CN2024/135144
International Filing Date
28.11.2024
Title **
[English]
PREPARATION METHOD FOR BIO-BASED POLYURETHANE ELASTIC FIBER
[French]
PROCÉDÉ DE PRÉPARATION DE FIBRES ÉLASTIQUES DE POLYURÉTHANE D'ORIGINE BIOLOGIQUE
[Chinese]
一种生物基聚氨酯弹性纤维的制备方法
Applicants **
JINJIANG ANRUN TEXTILE CO., LTD.
Inventors
XIAO, Jinbin
YIN, Honghui
Priority Data
202410620543.7
20.05.2024
CN
Application details
| Total Number of Claims/PCT | * |
| Number of Independent Claims | * |
| Number of Priorities | * |
| Number of Multi-Dependent Claims | * |
| Number of Drawings | * |
| Pages for Publication | * |
| Number of Pages with Drawings | * |
| Pages of Specification | * |
| * | |
| Number of Office Actions | * |
| * | |
International Searching Authority |
CNIPA
* |
| Recordal of a Change of the Applicant's Name/Address |
Change of Applicant's Name and Address
* |
| Type of Assignment |
The Standard Agent's Assignment
* |
| Applicant's Legal Status |
Legal Entity
* |
| * | |
| * | |
| * | |
| * | |
| * | |
| Entry into National Phase under |
Chapter I
* |
| Patent Delivery |
Send the Letters Patent by Courier
* |
| 译文 |
|
* The data is based on automatic recognition. Please verify and amend if necessary.
** IP-Coster compiles data from publicly available sources. If this data includes your personal information, you can contact us to request its removal.
Quotation for National Phase entry
| Country | Stages | Total | |
|---|---|---|---|
| China | Filing, Examination, Granting | 1576 | |
| EPO | Filing, Examination, Granting | 11576 | |
| Japan | Filing, Examination, Granting | 1846 | |
| South Korea | Filing, Examination, Granting | 1472 | |
| USA | Filing, Examination, Granting | 4740 |

Total:
21,210
Contact Us
Abstract[English]
The present invention relates to the field of the preparation of polyurethane elastic fibers, and relates to a preparation method for a bio-based polyurethane elastic fiber, comprising: preparing polyether polyol from sucrose, glycerol, dimethylamine and propylene oxide; adding a solvent, i.e., N,N-dimethylacetamide, and polyether polyol and polyisocyanate into a reaction tank, and adding p-Toluenesulfonyl semicarbazide and aluminum methylenebis(2,4-di-tert-butylphenoxy) phosphate to prepare a spinning solution; and subjecting the spinning solution to spinning and oil application by means of dry spinning technology to obtain the bio-based polyurethane elastic fiber. The present invention ensures that the properties of polyurethane elastic fibers do not deteriorate or are partially enhanced, while the cost and performance advantages are achieved.[French]
La présente invention concerne le domaine de la préparation de fibres élastiques de polyuréthane, et concerne un procédé de préparation d'une fibre élastique de polyuréthane d'origine biologique, comprenant : la préparation de polyol de polyéther à partir de saccharose, de glycérol, de diméthylamine et d'oxyde de propylène ; l'ajout d'un solvant, c'est-à-dire le N, N-diméthylacétamide, et le polyéther polyol et le polyisocyanate dans un réservoir de réaction, et l'ajout du p-toluènesulfonylsemicarbazide et du phosphate de méthylènebis(2,4-di-tert-butylphénoxy) d'aluminium pour préparer une solution de filage ; et à soumettre la solution de filage à un filage et à une application d'huile au moyen d'une technologie de filage à sec pour obtenir la fibre élastique de polyuréthane d'origine biologique. La présente invention garantit que les propriétés des fibres élastiques de polyuréthane ne se détériorent pas ou sont partiellement améliorées, tandis que les avantages de coût et de performance sont obtenus.[Chinese]
本发明涉及一种生物基聚氨酯弹性纤维的制备方法,属于聚氨酯弹性纤维制备领域,采用蔗糖、甘油、二甲胺、环氧丙烷制得聚醚多元醇;在反应罐中加入溶剂N,N‑二甲基乙酰胺、聚醚多元醇和多异氰酸酯,加入的对甲苯磺酰氨基脲和甲撑双(2,4‑二叔丁基苯氧基)磷酸铝制得纺丝原液;将纺丝原液通过干法纺丝技术,经纺丝、上油,制得生物基聚氨酯弹性纤维。本发明保证了聚氨酯弹性纤维性能不降低或部分功能提升,同时兼顾成本和性能优势。