WO2025027592 - A METHOD FOR MANUFACTURING AN ACTIVATED CARBON, SILVER-COFFEE GROUNDS COMPOSITE
National phase entry is expected:
Publication Number
WO/2025/027592
Publication Date
06.02.2025
International Application No.
PCT/ID2023/000008
International Filing Date
01.12.2023
Title **
[English]
A METHOD FOR MANUFACTURING AN ACTIVATED CARBON, SILVER-COFFEE GROUNDS COMPOSITE
[French]
PROCÉDÉ DE FABRICATION D'UN COMPOSITE DE CHARBON ACTIF ET D'ARGENT-MARC DE CAFÉ
Applicants **
BADAN RISET DAN INOVASI NASIONAL (BRIN)
Inventors
PRASETIA, Hafiizh
RAFIDAH, Haidar Sitie
KURNIAWAN, Hendris Hendarsyah
SAEFUMILLAH, Asep
ANNISA, Nova
Priority Data
P00202306985
31.07.2023
ID
Application details
| Total Number of Claims/PCT | * |
| Number of Independent Claims | * |
| Number of Priorities | * |
| Number of Multi-Dependent Claims | * |
| Number of Drawings | * |
| Pages for Publication | * |
| Number of Pages with Drawings | * |
| Pages of Specification | * |
| * | |
| Number of Office Actions | * |
| * | |
International Searching Authority |
MOIP
* |
| Recordal of a Change of the Applicant's Name/Address |
Change of Applicant's Name and Address
* |
| Type of Assignment |
The Standard Agent's Assignment
* |
| Applicant's Legal Status |
Legal Entity
* |
| * | |
| * | |
| * | |
| * | |
| * | |
| Entry into National Phase under |
Chapter I
* |
| Patent Delivery |
Send the Letters Patent by Courier
* |
| Translation |
|
* The data is based on automatic recognition. Please verify and amend if necessary.
** IP-Coster compiles data from publicly available sources. If this data includes your personal information, you can contact us to request its removal.
Quotation for National Phase entry
| Country | Stages | Total | |
|---|---|---|---|
| China | Filing, Examination, Granting | 1955 | |
| EPO | Filing, Examination, Granting | 11598 | |
| Japan | Filing, Examination, Granting | 1890 | |
| South Korea | Filing, Examination, Granting | 1302 | |
| USA | Filing, Examination, Granting | 4740 |

Total:
21,485
The term for entry into the National Phase has expired. This quotation is for informational purposes only
Contact Us
Abstract[English]
This invention relates to the manufacturing method for an activated carbon composite, specifically a silver and coffee grounds composite consisting of the following stages: preparing the waste coffee grounds, preparing AgNO3 solution, synthesizing the silver-coffee grounds composite, activating the silver-coffee grounds composite, washing the silver-coffee grounds composite, drying the silver-coffee grounds composite, pyrolyzing the silver-coffee grounds composite, washing the silver-coffee grounds composite, and drying the silver-coffee grounds composite material, which is conducted by: a) preparing the waste coffee grounds, b) preparing a 10 mM AgNO3 solution; C) synthesizing silver-coffee grounds composite using the wave irradiation method by mixing 25 ml of 10 mM AgNO3 with 50 ml of a coffee grounds solution; d) activating the silver-coffee grounds composite physically or chemically; e) washing the silver-coffee grounds composite material using hot distilled water to reach a neutral pH; f) drying the silver-coffee grounds composite material at 110°C in the oven for 2 to 3 hours; g) pyrolyzing the silver-coffee groundss composite for 1 hour at 500°C under nitrogen gas (N2); h) washing the silver-coffee grounds composite using hot distilled water to a neutral pH; and i) drying the silver-coffee grounds composite at 110°C in the oven for 2 to 3 hours.[French]
La présente invention concerne le procédé de fabrication d'un composite de charbon actif, en particulier un composite d'argent et de marc de café constitué des étapes suivantes : préparer le marc de café usagé, préparer une solution d'AgNO3, synthétiser le composite d'argent-marc de café, activer le composite d'argent-marc de café, laver le composite d'argent-marc de café, sécher le composite d'argent-marc de café, pyrolyser le composite d'argent-marc de café, laver le composite d'argent-marc de café, et sécher le matériau composite d'argent-marc de café, qui est conduit par : a) préparer le marc de café usagé, b) préparer une solution d'AgNO3 de 10 mM; c) synthétiser un composite d'argent-marc de café à l'aide du procédé d'irradiation d'onde par mélange de 25 ml d'AgNO3 de 10 mM avec 50 ml d'une solution de marc de café; d) activer physiquement ou chimiquement le composite d'argent-marc de café; e) laver le matériau composite d'argent-marc de café à l'eau distillée chaude pour obtenir un pH neutre; f) sécher le matériau composite d'argent-marc de café à 110°C dans le four pendant 2 à 3 heures; g) pyrolyser le composite d'argent-marc de café pendant 1 heure à 500°C sous azote gazeux (N2); h) laver le composite d'argent-marc de café à l'eau distillée chaude à un pH neutre; et i) sécher le composite d'argent-marc de café à 110°C dans le four pendant 2 à 3 heures.