WO2026053076 - MARINE WATER AS HYDRATION AGENT FOR REACTIVE MAGNESIUM OXIDE CEMENT
National phase entry is expected:
Publication Number
WO/2026/053076
Publication Date
12.03.2026
International Application No.
PCT/IB2025/058707
International Filing Date
28.08.2025
Title **
[English]
MARINE WATER AS HYDRATION AGENT FOR REACTIVE MAGNESIUM OXIDE CEMENT
[French]
EAU DE MER EN TANT QU'AGENT D'HYDRATATION POUR CIMENT D'OXYDE DE MAGNÉSIUM RÉACTIF
Applicants **
NEW YORK UNIVERSITY IN ABU DHABI CORPORATION
Inventors
CELIK, Kemal
WANG, Xiangyu
KRISHNAN, Padmaja
Priority Data
63/690,189
03.09.2024
US
Application details
| Total Number of Claims/PCT | * |
| Number of Independent Claims | * |
| Number of Priorities | * |
| Number of Multi-Dependent Claims | * |
| Number of Drawings | * |
| Pages for Publication | * |
| Number of Pages with Drawings | * |
| Pages of Specification | * |
| * | |
| Number of Office Actions | * |
| * | |
International Searching Authority |
MOIP
* |
| Recordal of a Change of the Applicant's Name/Address |
Change of Applicant's Name and Address
* |
| Type of Assignment |
The Standard Agent's Assignment
* |
| Applicant's Legal Status |
Legal Entity
* |
| * | |
| * | |
| * | |
| * | |
| * | |
| Entry into National Phase under |
Chapter I
* |
| Patent Delivery |
Send the Letters Patent by Courier
* |
| Translation |
|
* The data is based on automatic recognition. Please verify and amend if necessary.
** IP-Coster compiles data from publicly available sources. If this data includes your personal information, you can contact us to request its removal.
Quotation for National Phase entry
| Country | Stages | Total | |
|---|---|---|---|
| China | Filing, Examination, Granting | 2099 | |
| EPO | Filing, Examination, Granting | 11600 | |
| Japan | Filing, Examination, Granting | 2181 | |
| South Korea | Filing, Examination, Granting | 1659 | |
| USA | Filing, Examination, Granting | 4740 |

Total:
22,279
Contact Us
Abstract[English]
The systems and methods include a method. The method can include mixing, for a first time period, salt water with reactive magnesium oxide cement (RMC) at a first ratio to create a first mixture. The method can include mixing, for a second time period, the first mixture with an aggregate at a second ratio to create a second mixture. The method can include hydrating, for a third time period, the second mixture by molding and covering the second mixture. The method can include curing, for a fourth time period, the second mixture in a chamber to create an RMC-based composite, the chamber having a temperature value, a humidity value, and a CO2 concentration value.[French]
Les systèmes et les procédés selon l’invention comprennent un procédé. Le procédé peut comprendre le mélange, pendant une première période, d'eau salée avec du ciment d'oxyde de magnésium réactif (RMC) à un premier rapport pour former un premier mélange. Le procédé peut comprendre le mélange, pendant une deuxième période, du premier mélange avec un agrégat à un deuxième rapport pour former un deuxième mélange. Le procédé peut comprendre l'hydratation, pendant une troisième période, du deuxième mélange par moulage et recouvrement du deuxième mélange. Le procédé peut comprendre le durcissement, pendant une quatrième période, du deuxième mélange dans une chambre pour créer un composite à base de RMC, la chambre ayant une valeur de température, une valeur d'humidité et une valeur de concentration de CO2.