WO2026097978 - LIGNIN-MODIFIED WATERBORNE POLYURETHANE STRIPPABLE COATING AND PREPARATION METHOD THEREFOR
National phase entry is expected:
Publication Number
WO/2026/097978
Publication Date
15.05.2026
International Application No.
PCT/CN2025/113481
International Filing Date
08.08.2025
Title **
[English]
LIGNIN-MODIFIED WATERBORNE POLYURETHANE STRIPPABLE COATING AND PREPARATION METHOD THEREFOR
[French]
REVÊTEMENT PELABLE EN POLYURÉTHANE À BASE AQUEUSE MODIFIÉ PAR DE LA LIGNINE ET SON PROCÉDÉ DE PRÉPARATION
[Chinese]
一种木质素改性水性聚氨酯可剥离涂料及其制备方法
Applicants **
CNOOC CHANGZHOU PAINT AND COATINGS INDUSTRY RESEARCH INSTITUTE CO., LTD.,
CNOOC CHANGZHOU ENVIRONMENTAL PROTECTION COATING CO., LTD
Inventors
WANG, Yaxin
CAO, Yacheng
WU, Ming
SHI, Liping
CHEN, Li
Priority Data
202411587360.6
08.11.2024
CN
Application details
| Total Number of Claims/PCT | * |
| Number of Independent Claims | * |
| Number of Priorities | * |
| Number of Multi-Dependent Claims | * |
| Number of Drawings | * |
| Pages for Publication | * |
| Number of Pages with Drawings | * |
| Pages of Specification | * |
| * | |
| Number of Office Actions | * |
| * | |
International Searching Authority |
CNIPA
* |
| Recordal of a Change of the Applicant's Name/Address |
Change of Applicant's Name and Address
* |
| Type of Assignment |
The Standard Agent's Assignment
* |
| Applicant's Legal Status |
Legal Entity
* |
| * | |
| * | |
| * | |
| * | |
| * | |
| Entry into National Phase under |
Chapter I
* |
| Patent Delivery |
Send the Letters Patent by Courier
* |
| Translation |
|
* The data is based on automatic recognition. Please verify and amend if necessary.
** IP-Coster compiles data from publicly available sources. If this data includes your personal information, you can contact us to request its removal.
Quotation for National Phase entry
| Country | Stages | Total | |
|---|---|---|---|
| China | Filing, Examination, Granting | 1576 | |
| EPO | Filing, Examination, Granting | 11761 | |
| Japan | Filing, Examination, Granting | 2010 | |
| South Korea | Filing, Examination, Granting | 1710 | |
| USA | Filing, Examination, Granting | 4740 |

Total:
21,797
Abstract[English]
Disclosed in the present invention are a lignin-modified waterborne polyurethane strippable coating and a preparation method therefor. The strippable coating is obtained by sequentially reacting and mixing a waterborne epoxy ester modified carbon dioxide-based polyurethane, a functionalized lignin/silicon dioxide filler, a color paste, a defoaming agent, an anti-sticking agent, a thickening agent and deionized water. In the lignin-modified waterborne polyurethane strippable coating prepared in the present invention, a matrix resin and the filler are subjected to relatively comprehensive molecular structure modification, and the cross-linked structure of a coating is significantly changed, such that an epoxy ester and a carbon dioxide-based polyol are introduced, and the cross-linked density of a prepared coating film is significantly improved; in addition, the introduction of the functionalized lignin/silicon dioxide improves the outdoor aging resistance and corrosion resistance of the coating, and the strippable performance of a paint film, which has been exposed to the outdoors for two years, is still very excellent.[French]
La présente invention divulgue un revêtement pelable en polyuréthane à base aqueuse modifié par de la lignine et son procédé de préparation. Le revêtement pelable est obtenu par réaction séquentielle et mélange d'un polyuréthane à base de dioxyde de carbone modifié par un ester époxy à base aqueuse, d'une charge de lignine fonctionnalisée/dioxyde de silicium, d'une pâte colorée, d'un agent antimousse, d'un agent antiadhésif, d'un agent épaississant et d'eau désionisée. Dans le revêtement pelable en polyuréthane à base aqueuse modifié par de la lignine préparé selon la présente invention, une résine matrice et la charge sont soumises à une modification de structure moléculaire relativement complète, et la structure réticulée d'un revêtement est significativement modifiée, de telle sorte qu'un ester d'époxy et un polyol à base de dioxyde de carbone sont introduits, et la densité réticulée d'un film de revêtement préparé est considérablement améliorée ; de plus, l'introduction de la lignine fonctionnalisée/du dioxyde de silicium améliore la résistance au vieillissement et la résistance à la corrosion en extérieur du revêtement, et la performance pelable d'un film de peinture, qui a été exposé à l'extérieur pendant deux ans, est encore assez excellente.[Chinese]